Fig. 7
From: Recycling of aluminum dross for producing calcinated alumina by microwave plasma

XRD pattern of SAD residue after under different CNaOH (reacted at 50 °C, 60 min)
From: Recycling of aluminum dross for producing calcinated alumina by microwave plasma
XRD pattern of SAD residue after under different CNaOH (reacted at 50 °C, 60 min)