From: Recovery and purification of kish graphite from steelmaking dust by using acid leaching with physical auxiliary methods
Auxiliary method
Temperature (°C)
Carbon content (wt%)
0.3 N HCl
1.0 N HCl
None
ambient
93.13
95.06
Heating
60
93.37
95.37
80
94.08
97.06
100
94.22
Microwave irradiation
40
90.65
96.15
91.49
96.54
94.84
96.50