From: Recovery and purification of kish graphite from steelmaking dust by using acid leaching with physical auxiliary methods
Amplitude
(%)
Reaction time
(min)
Input energy
(kJ)
Temperature
(°C)
Carbon content (wt%)
25
5
8.7
55
91.20
50
14.9
69
92.78
75
0.5
2.2
32
89.71
1
4.3
39
91.73
2
8.4
53
93.86
18.6
67
93.95
30
63.3
78
94.53